Überrollungslebensdauer des Wälzlagerstahls100Cr6 in Abhängigkeit von nicht idealenGefügeausbildungen unter besondererBerücksichtigung der Karbidzeiligkeit
File | Description | Size | Format | |
---|---|---|---|---|
00011800.pdf | 34.99 MB | Adobe PDF | View/Open |
Other Titles: | Rolling contact fatigue life of steel 100Cr6 depending on non-ideal microstructures especially carbide strings | Authors: | Burkart, Klaus | Supervisor: | Zoch, Hans-Werner | 1. Expert: | Zoch, Hans-Werner | Experts: | Eifler, Dietmar | Abstract: | In this study rolling contact fatigue life tests of different variants of 100Cr6 (SAE 52100) bearing steel were performed with roller bearings under hydrodynamic lubrication. All bearings failed from subsurface crack initiation. Additionally determined fatigue lives gained from compression torsion tests with round specimens could be correlated with the results of the rolling contact fatigue tests. Carbide strings resulting from primary carbides are locally concentrated in the core of the semi-finished material where the non-metallic inclusion content is also increased. Generally, carbide strings may have a negative influence on the fatigue life behaviour. If present in regions of highly stressed material in the bearings oxides are the life limiting factor of rolling contact fatigue life. |
Keywords: | rolling contact fatigue; crack initiation; carbide strings | Issue Date: | 4-Dec-2009 | Type: | Dissertation | Secondary publication: | no | URN: | urn:nbn:de:gbv:46-diss000118004 | Institution: | Universität Bremen | Faculty: | Fachbereich 04: Produktionstechnik, Maschinenbau & Verfahrenstechnik (FB 04) |
Appears in Collections: | Dissertationen |
Page view(s)
420
checked on Apr 3, 2025
Download(s)
1,920
checked on Apr 3, 2025
Google ScholarTM
Check
Items in Media are protected by copyright, with all rights reserved, unless otherwise indicated.