Now showing 1 - 10 of 69
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Prevention of coating-induced agglomerations within the weld seam during laser beam deep penetration welding of aluminum-silicon coated press-hardened steel
    Press-hardened steels like 22MnB5 (1.5528) have great potential in terms of their use in the field of lightweight construction. However, due to the aluminum-silicon coating, applied for press-hardening, strength-reducing agglomerations can occur within the seam after laser deep penetration welding of already hardened material. To investigate the hypothesis that the agglomeration formation can be reduced by beam modulation strategies, laser deep penetration welding experiments with changing beam modulation strategies such as “transversal”, “circular” and “vertical eight” shaped patterns were carried out using constant welding speed and laser power. After comparing the resulting cross-sections to coated and decoated samples welded without beam modulation, the hypothesis was found to be true in case of all modulation strategies examined as no agglomerations could be detected within the samples. In addition, in case of the beam modulation strategies “circle” and “vertical eight”, the fracture type could be changed from a separation fracture along the melting line to a shear fracture crosswise to the seam in sheet metal plane comparable to the decoated samples.
    journal article
      349  157
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Tribological system for cold sheet metal forming based on volatile lubricants and laser structured surfaces
    A novel tribological system has been developed, in which volatile lubricants (carbon dioxide - CO2 or nitrogen- N2) are used as a substitute for mineral oil-based lubricants in deep drawing processes. This process enables the introduction of an intermediate medium under high pressure through flow-optimized, laser-drilled micro holes into the contact surfaces. This eliminates the need for subsequent, cost-intensive cleaning processes, as the volatile lubricants evaporate without leaving any residue during expansion to ambient pressure. The design of initial micro hole geometries was based on simulations of the flow behaviour of the lubricants passing through, which in turn were validated using pressure reactor tests. In addition, the wetting behaviour of CO2 on relevant surfaces (tool surface and sheet material surface) was investigated experimentally using the captive-bubble-method. Thus, the optimal design of the micro holes (diameter, hole geometry and number of micro holes) could be determined using flat strip drawing tests. The optimal micro hole geometry determined in this way is suited for the use of both CO2 and N2 as volatile lubricant. Furthermore, extensive investigations for the production of the required micro hole geometry by laser drilling were carried out. The fundamentals for drilling micro holes in steel with high aspect ratios could be developed using an ultrashort pulsed research laser with very high pulse energy. Further experiments were conducted using an ultrashort pulsed prototype laser of the kW-class specially developed to increase productivity when drilling a multitude of micro holes with higher average laser power. The novel tribological system has been characterised by means of strip drawing tests and stretch bending tests. For both, CO2 (liquid) and N2 (gaseous), relatively low friction values could be achieved compared to conventional lubricants. It could be shown that deep drawing with both CO2 and N2 as dry lubricants is possible. Here, usage of the volatile lubricants not only allows the replacement of mineral oil based lubricants, but even improves the tribological system with regard to frictional forces in sheet metal forming. The feasibility of the new tribological system has been proven by performing deep drawing tests of rectangular cups. These tests showed a significantly enlarged process window of the forming process, which emphasise the tremendous potential of this new tribological system.
    journal article
      756  362
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Macro- and microstructuring of deep drawing tools for dry forming processes
    In forming processes, lubrication is needed to reduce friction and wear occurring at the contact areas between the work-piece and the tool. This is provided by separating these surfaces as well as transporting abrasive wear out of the sliding interface. With high interest in waste avoidance and efficient use of resources, today’s industry aims for substituting these lubricants. Thereby, deposition of coatings or local surface structuring offer a different way to reduce friction in forming processes. For instance, this can be reached by using different hard coatings as well as by utilizing manufacturing methods capable to control and reduce the contact area in the tribological system. In this project, the flange area of a deep drawing tool was macro-structured by turning-process (rotational symmetric geometry) and by milling-process (non rotational-symmetric part) to decrease the contact area of the work-piece up to 94% during the forming process. Also, the drawing edge radius of the tools was coated with different types of hydrogen-free tetrahedral amorphous carbon layers, e.g. with a sp³-ratios between 60% and 70%. Together with the subsequently introduced micro-features on the ta-C layer, employing the innovative method of Direct Laser Interference Patterning (DLIP), a further reduction of the contact areas was possible as well as to produce local rehybridization of the ta-C material. Also, high-throughput surface texturing of semi-finished sheet metals by DLIP process was performed, for reducing friction by minimizing also the contact area with the deep drawing tool. Forming of test strips showed the influence of the macro-structured flange area by reducing the friction force down to 75%. In addition, different modelling tools were developed for calculating both the process window and to determine the generation of wrinkles during deep drawing with macro-structured tools. The macro-structured deep drawing tools could also enlarge the process limits by increasing the stability against wrinkling of the sheet metal during the drawing process. The ta-C coating on the die radius without application of lubrication was capable to reduce the friction coefficient up to 20% compared to uncoated lubricated conditions. Performed tensile-bend tests on micro-structured ta-C coated cylinders also demonstrated the potential to reduce friction, as well as an excellent capability to reduce wear compared to the standard conditions.
    journal article
      558  386
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Improved 3D form profiler based on extending illumination aperture
    (Society of Photo‑Optical Instrumentation Engineers (SPIE), 2023-08-15) ; ;
    We recently demonstrated that the 3D shape of micro-parts can be measured using LED illumination based on contrast evaluation. The technique is based on imaging the object under test using partially coherent illumination. The limited spatial coherence of LED illumination was utilized to discriminate depth. For a fast depth scan without mechanically moving parts, an electrically tunable lens (ETL) in a 4f optical configuration is used. This approach is efficient, takes less than a second to capture all required images, is eye-safe, and offers a depth of focus of a few millimeters. However, the main limitation of the proposed approach arises from the underlying assumption that a small angle of variation of illumination is required. Such a small illumination aperture affects the axial scan resolution that dominates the measurement uncertainty. In the present paper we propose a method to overcome the main limitation of the above-mentioned profiling technique. The approach combines measurements with multiple illumination directions achieved by illuminating the object simultaneously with several independent light sources. In this way, the full-width half maximum of the contrast envelope is reduced. A tilted metallic plate is used for proof of concept.
    conference paper
      32  85
  • Some of the metrics are blocked by your 
    Item type:Publication,
    LAF 2022: Proceedings of the 12th Laser Applications Forum
    Current R&D at BIAS is highlighted in a special session at LAF 2022, and a collection of respective short papers from BIAS is published in this proceedings volume, freely available via open access.
    Book
    Band:
      462  296
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Lokale Beeinflussung der Oberflächenrauheit von Silizium dotiertem CVD-Diamant durch funkenerosive Mikrobearbeitung
    (2016) ; ;
    Prieske, Markus
    ;
    Zeidler, Henning
    ;
    Schubert, Andreas
    CVD-Diamantschichten besitzen ein hohes Potential für den Einsatz als verschleißfeste Oberflächen-beschichtungen für Umformwerkzeuge. Zur Vermeidung von Beschädigungen am Werkstück im Umformprozess sind geringe Oberflächen-rauheiten gefordert. Polykristalline CVD-Diamantschichten bestehen aus einzelnen Diamantkristallen, welche im Be-schichtungsprozess zusammenwachsen. Die einzelnen Diamantkristalle führen dabei zu einer erhöhten Oberflächenrau-heit, sodass eine Nachbearbeitung zum Glätten dieser ultraharten Schichten notwendig wird. Eine Herausforderung stellt insbesondere die lokale Veränderung der Oberfläche dar, welche zur Funktionalisierung dieser Schichten beitragen kann. Ein geeignetes Verfahren zur lokalen Beeinflussung stellt die Mikrofunkenerosion (Mikro-EDM) dar, welche als kon-taktfreies Fertigungsverfahren, unabhängig von den mechanischen Eigenschaften des Werkstoffes, eine Bearbeitung er-möglicht. Eine wichtige Einschränkung stellt die erforderliche elektrische Mindestleitfähigkeit von 0,01 Ω-1cm-1 dar, wes-halb das Verfahren ausschließlich für dotierte CVD-Diamantschichten einsetzbar ist. Im Rahmen dieser Veröffentlichung wird eine Möglichkeit vorgestellt, die Oberflächenrauheit einer mit Silizium dotier-ten CVD-Diamantschicht durch Mikro-EDM lokal zu beeinflussen. Dazu wurde durch Bahnerosion mit einer Stabelekt-rode (ø 90 μm) ein Feld mit den Abmessungen von 500 μm x 250 μm bearbeitet. Anschließend wurde die Oberfläche qualitativ und quantitativ durch Laserscanning-Mikroskopie analysiert. Die Oberflächenrauheit Sa konnte von 1,43 μm auf 0,83 μm reduziert, sowie die reduzierte Spitzenhöhe Spk um 78% verringert werden.
    journal article
    Band:
      538  130
  • Some of the metrics are blocked by your 
    Item type:Publication,
    High-speed laser melt injection for wear protection of skin-pass rolls
    Laser melt injection (LMI) is a technology for producing metal matrix composite (MMC) layers on tools such as skin-pass rolls by injecting hard particles into a laser-induced weld pool. However, low process speeds prevent the application of laser melt injection on a large scale. To overcome this drawback, a new approach is presented: High-speed laser melt injection (HSLMI) is a promising method for generating highly wear-resistant MMC-layers on tools with high productivity. For the first time, high process speeds of up to 100 m/min were reached with HSLMI of spherical fused tungsten carbide (SFTC) particles into the steel 1.2362 that is used for skin-pass rolls. It was found that both the crack susceptibility and the SFTC dissolution can be reduced significantly by increasing the process speed. The wear behavior of the MMC layers was studied in a pin-on-plate test. It was found that the SFTC reinforcement leads to a significant improvement in wear resistance over the non-reinforced steel substrate. The wear volume was reduced from 3.6 mm³ to 0.1 mm³ to 0.3 mm³ by an SFTC particle-reinforcement.
    journal article
      289  230
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Einfluss von Metalldampf auf den Schweißlichtbogen
    Die Lichtbogenstabilität verbessert sich durch die Kombination des Lichtbogenschweißens mit dem Laserstrahlschweißprozess im Laserstrahl-Lichtbogen- Hybridschweißen. Der laserinduzierte Metalldampf wird dabei als stabilisierender Faktor betrachtet. Zur Untersuchung der Mechanismen, insbesondere des Einflusses des Metalldampfs, wurde eine experimentelle, orthogonale Prozesskombination eingesetzt. Diese Methode ermöglichte es, andere Einflüsse des Hybridprozesses zu minimieren. Die Ergebnisse zeigten eine Destabilisierung des Lichtbogens durch den laserinduzierten Metalldampfeinfluss. Die Destabilisierung resultierte aus der Summe negativer Einflüsse auf die Lichtbogenleitfähigkeit in der verwendeten Prozesskombination. Im realen Hybridprozess wird aufgrund günstigerer Bedingungen eine Stabilisierung erwartet.
    doctoral thesis
    Band:
      51  121
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Hochgeschwindigkeits-Laserdispergieren zur Erzeugung funktionaler MMC-Randschichten
    Beim Laserdispergieren werden Metallmatrix-Verbundwerkstoff (MMC)-Schichten erzeugt, indem ein pulverförmiger Hartstoff in ein durch einen Laserstrahl induziertes Schmelzbad gefördert wird. Die vorliegende Arbeit befasst sich mit den Mechanismen während des Hartpartikelflugs und der -inkorporation im Schmelzbad sowie der gezielten Beeinflussung dieser Mechanismen mit dem Ziel, eine Bearbeitung mit Prozessgeschwindigkeiten oberhalb von 5 m/min zu ermöglichen. Ein zentrales Kriterium ist dabei die Reduktion von Interaktionen zwischen Hartpartikeln und dem Laserstrahl, die zu einem unerwünschten Aufschmelzen von Hartpartikeln führen können. Zudem wird gezeigt, dass durch eine Erhöhung der Prozessgeschwindigkeit Defekte der MMC- Schicht wie Poren und Hartstoffauflösungen deutlich reduziert werden können. Im Rahmen von zwei Beispielen – Dressierwalzen und Druckgusskolben – werden neue Anwendungsmöglichkeiten des Hochgeschwindigkeits-Laserdispergierens demonstriert.
    doctoral thesis
    Band:
      100  65
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Selective oxidation of 1.2379 tool steel surfaces : an approach for Dry Metal Forming
    (2015) ;
    Yilkiran, Deniz
    ;
    Holländer, Ulrich
    ;
    Lützenkirchen-Hecht, Dirk
    ;
    Wagner, Ralph
    Subject of this work is the development of a simple and cost-efficient process for conditioning the surface of forming tools for deep drawing processes in order to minimize friction and wear to a level that dry forming processes without any lubricants will be possible in future. The approach chosen is an oxidative heat treatment of the tool surfaces at controlled oxygen partial pressures and temperatures. Thus, alloying elements of the tool shall constitute oxide layers with advantageous tribological properties suitable for the aimed application. In this paper results from parameter studies concerning the controlled surface oxidation of a hardened conventional tool steel (EU alloy grade 1.2379 X153CrMoV12) are presented. Beside the dependence of the oxide layer morphology from the chosen heat treatment parameters first results of their tribological behavior gained from measurements of the friction coefficients using an application-oriented strip drawing test are presented. From these investigations promising results and conclusions for future work have been obtained which are discussed in the paper
    journal article
    Band:
      449  194