Schmiedegerecht nitrierte Gesenke
File | Description | Size | Format | |
---|---|---|---|---|
00106106-1.pdf | 30.23 MB | Adobe PDF | View/Open |
Other Titles: | Nitrided forging dies | Authors: | Hoja, Stefanie | Supervisor: | Hoffmann, Franz | 1. Expert: | Hoffmann, Franz | Experts: | Keßler, Olaf | Abstract: | In order to resist the high loads, the surfaces and boundary areas of forging dies are nitrided. Up to now, there was no proven knowledge about, which processing parameters respectively which nitrided case leads to the best life time of the tools. In the present work, the influence of nitriding and nitrocarburizing with all their variety of nitrided cases on the lifetime and wear of forging dies was investigated. Eight promising treatments were transferred to forging dies, in order to create a number of different nitrided cases. The tools were used in serial production and their lifetime was determined under real conditions. At the lifetime end, critical parts of the tools were metallographical investigated, in order to find out the wear mechanisms. Finally, a recommendation was developed which nitrided case revealed the best results for a given loading condition. |
Keywords: | Nitriding; Nitrocarburizing; X38CrMoV5-3; Forging dies | Issue Date: | 23-Aug-2017 | Type: | Dissertation | Secondary publication: | no | URN: | urn:nbn:de:gbv:46-00106106-13 | Institution: | Universität Bremen | Faculty: | Fachbereich 04: Produktionstechnik, Maschinenbau & Verfahrenstechnik (FB 04) |
Appears in Collections: | Dissertationen |
Page view(s)
347
checked on Mar 28, 2024
Download(s)
134
checked on Mar 28, 2024
Google ScholarTM
Check
Items in Media are protected by copyright, with all rights reserved, unless otherwise indicated.