Now showing 1 - 7 of 7
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Multifunctional hyperbranched prepolymers with tailored degree of methylation and methacrylation
    A synthesis approach for multifunctional crosslinkable hyperbranched prepolymers with tailored degree of methylation and methacrylation with full conversion of all hydroxyl groups was investigated. Prepared by catalyzed esterification various methacrylate substitution degrees could be adjusted using predefined partially methylated polyglycerol-based precursors. The combination of methacrylic anhydride, triethylamine and 4-dimethylaminopyridine was proven to be beneficial for the esterification and full conversion of the remaining primary as well as secondary hydroxyl groups. NMR, IR and Raman spectroscopy were used to prove the insertion of methacrylic crosslinking groups in the polymeric backbone. The obtained prepolymers can be photopolymerized in bulk, while a higher methacrylate content leads to a higher crosslink density after UV curing resulting in higher stiffness and higher glass transition temperature. Atomistic model simulation clarified spatial structure of the crosslinked macromolecules and allowed Tg predictions. Viscoelastic to ideal-viscous behaviour dominates in the obtained polymeric products with low network density.
    journal article
    Band:
      41  77
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Synthesis and characterization of hyperbranched polyglycerols with various degree of methylation employing phase-transfer conditions
    A simple method for partial methylation of the hyperbranched polyglycerol hydroxyl groups was achieved by a combination of phase-transfer catalysis approach with dimethyl sulfate and tetrabutylammonium bromide and the use of a mixed-bed ion exchanger for purification. Various degrees of methylation between 0 and 98% could be adjusted in a controlled manner via the added amount of alkylating agent resulting in modified polymers with moderate polydispersities. NMR spectroscopy was used to determine the methylation progress and the resulting molecular structure. The methylation degree affected associative intra- and intermolecular interactions, such as hydrogen bonds, entailing reduced glass transition temperature and viscosities with increasing hydroxyl group conversion. In addition, the attenuation of hydrogen bonds upon methylation proved to facilitate a straightforward estimation of methylation degree by infrared spectroscopy.
    journal article
    Band:
      19  23
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Polyoxopalladate-Loaded Metal–Organic Framework (POP@MOF): Synthesis and Heterogeneous Catalysis
    We report on the synthesis and characterization of the first polyoxo-noble-metalate-containing metal–organic framework (MOF) material, wherein the preformed MIL-101 has been impregnated with the discrete, cuboid-shaped polyoxopalladate [Pd13Se8O32]6– (Pd13Se8), leading to the composite Pd13Se8@MIL-101. This material was characterized by FTIR, TGA, elemental analysis, powder-XRD, N2 sorption (BET), SEM-EDX, and XPS. Furthermore, the Pd13Se8@MIL-101 composite was shown to be an effective, stable, and recyclable heterogeneous precatalyst for the Suzuki−Miyaura cross-coupling reaction at room temperature utilizing environmentally benign solvents, such as water and methanol.
    journal article
    Band:
    Heft:
      21  46
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Secondary dispersion-based reactive pressure-sensitive adhesives with improved tack
    Reactive pressure-sensitive adhesives (PSA) have to meet the requirements for sufficient tack prior to crosslinking but also high shear after crosslinking. This article examines the use of secondary acrylic dispersions with reactive groups and epoxy resin dispersions for such PSA. Long-term stable secondary PSA dispersions with high tack after film formation were obtained. Tack was dependent on the amount of carboxylic acid groups in the polymer as well as the base used for partial neutralization of the solvent-borne copolymers. Reactive PSA were prepared by mixing a secondary dispersion with high amounts of carboxylic acid groups with an epoxy resin dispersion providing no tack. Variation of mixing ratio gave reactive PSA with sufficient tack, peel, and shear prior to crosslinking. Crosslinking of these reactive PSA at elevated temperatures led to high shear which was limited by incomplete molecular mixing of both phases. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018, 135, 46315.
    journal article
      126  215
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Influence of high-temperature and high-humidity aging on the material and adhesive properties of addition curing silicone adhesives
    Silicones are commonly used as sealants when high-performance materials are required due to harsh environmental conditions. To ensure a proper sealing function, the buildup of adhesion to the adherends is a prerequisite that is often addressed by the addition of adhesion promoters. However, the investigation of the fundamental adhesion mechanisms of silicones has been widely neglected. This work focuses on adhesive bond properties with aluminum adherends without the usage of adhesion promoters. The influence of high-temperature and high-humidity aging on the adhesive bond and material properties is examined. For this purpose, we formulated an addition curing silicone adhesive with a known composition. Aging took place for up to 56 d at different temperatures ranging from room temperature to 150 °C. In addition, we examined the influence of moisture by applying high-humidity conditions (85 °C/85% relative humidity). Changes in bulk material properties were characterized by stress at break, strain at break, Shore A hardness and swelling degree. Moreover, Fourier-transform infrared (FTIR) spectroscopy provided information about the chemical processes. The adhesive properties were determined using lap-shear joints. At high-temperature aging, the strain at break decreases while the hardness of the bulk material increases. A lower degree of swelling suggests an increasing cross-linking density. At the same time, lap-shear strengths increase and cohesive fracture patterns indicate a substantial buildup of adhesion. The samples aged under high-humidity conditions show a more complicated behavior. The increase in cross-linking density proceeds slower compared to high-temperature conditions (130 °C and 150 °C) but reaches higher values after 56 d. Lap-shear strengths tend to be lower compared to high-temperature storage and are accompanied by a significant amount of adhesive failure. FTIR spectroscopy reveals reactions of the residual hydrosiloxane groups of the cross-linking agent. However, these reactions are insufficient to fully explain the observed behavior. Therefore, reactions of the siloxane backbone are suggested. Although no specific adhesion promoters were used, high-temperature conditions enabled a substantial adhesion buildup of addition curing silicones on aluminum adherends under dry conditions. In contrast, humid conditions disturb adhesion buildup and are rather unfavorable for adhesion.
    journal article
      170  333
  • Some of the metrics are blocked by your 
    Item type:Publication,
    An in vitro bone-to-bone adhesion test method using the compression shear test
    The development of new bone adhesives is severely restricted due to the lack of a standard test method to examine their bond strength. Therefore, this study presents an in vitro bone-to-bone adhesion test method based on a compression shear test using cortical bone specimens (35 × 15 × 3 mm). The zero-gap lap joint test configuration was used to measure the bonding strengths of two soft tissue adhesives (Histoacryl® and BSA-Glue) and a bone cement (Palacos® LV). For reproducible bonding results, it is crucial to work with specimen having reproducible surface, dimensions and where and how they were taken from a bone. Therefore, this is a focus of the work. The adhesive strengths were determined under dry and physiological conditions to evaluate the reliability of the test procedure. Furthermore, the influence of previous acid etching of the bone surface was also investigated. The adhesives achieved bond strengths of 5.5 MPa (Histoacryl®), 3.2 MPa (BSA-Glue) and 2.8 MPa (Palacos® LV) under dry conditions. Under physiological conditions, the measured adhesive strengths of all three bonding materials decreased by around 90%. The acid etching led to a higher presence of reactive amino groups on the bone surface and improved the adhesion of Histoacryl® and BSA-Glue. The Palacos® LV bone cement suffered a reduction in adhesion as the acid smoothened the bone surface, resulting in less mechanical interlocking. The proposed test method is based on known standards and enables the usability of medical adhesives as a bone adhesive to be evaluated in a reproducible manner.
    journal article
    Band:
      25  46
  • Some of the metrics are blocked by your 
    Item type:Publication,
    Strong and super tough: Layered ceramic-polymer composites with bio-inspired morphology
    Bio-inspired layered ceramic-polymer composites with high strength and toughness were prepared from sintered aluminum oxide ceramic sheets and cationically curing epoxy resins toughened with poly(ε-caprolactone) (PCL). The architecture of the composite is inspired by nacre but is arranged on a larger scale. Ceramic sheets with a nominal thickness of 250 μm were assembled into composite plates by adhesive layers with a nominal thickness of 20 μm. Before the manufacturing of the composites, the stress-strain properties of the polymer component were tailored by the variation in the PCL content between 0 and 39 wt%. For composites with 4 and 15 ceramic layers, the bending strengths achieved 327 MPa and 376 MPa, which are higher than that of pure ceramic sheets. Moreover, composites with 15 ceramic layers show a 16 times higher toughness compared to that of the pure ceramic sheets. The results indicate that the toughness of the layered composites increases significantly with the number of layers. Inspired by the geometrical ratio of the natural sheet composite nacre, we have achieved a similar strength but a 2 times higher toughness than nacre by only adding up to 6 vol% of the polymer.
    journal article
      199  284